SESK: Stuff Everyone Should Know · sesk.info/weld-tig-tungsten-point
A ground tungsten point should be how long compared with its diameter?
About two and a half times the diameter.
- About the same as its diameter
- About 2.5 times its diameter ✔
- About 10 times its diameter
Why: A sharpened tungsten gives a focused arc. Miller says to grind it with a fine wheel used only for tungsten, so it stays uncontaminated.
Huh, didn't know that: Miller advises a 200 grit or finer wheel.
What did the triangle say to the circle? "You're pointless."
Like this card?
References
Answer: About 2.5 times its diameter. A sharpened tungsten gives a focused arc. Miller says to grind it with a fine wheel used only for tungsten, so it stays uncontaminated.
- Guide to TIG Welding Basics (Miller) www.millerwelds.com/en-US/resources/knowledge-hub/tig-welding/how-to/guide-to-tig-welding-basics
make the point roughly two and a half times as long as the diameter.
Checked 2026-10-10.
Think this answer is wrong? Tap "Challenge this answer" on the card in the game and tell us why.
More stuff everyone should know
That's stuff everyone should know.